HDPE(高密度聚乙烯#低压乙烯)/EGDA-6888/科威特EQUATE
原料技术数据
|
性能项目 |
试验条件[状态] |
测试方法 |
测试数据 |
数据单位 |
|
|
基本性能 |
熔体流动速率 |
190°C,2.16kg |
ASTM D-1238 |
0.05/9 |
dg/min |
|
密度 |
|
ASTM D-1505 |
0.952 |
g/cm3 |
|
|
物理性能 |
光泽度 |
45℃ |
ASTM D-2457 |
20 |
% |
|
机械性能 |
薄膜拉伸强度 |
MD |
ASTM D-882 |
52 |
MPa |
|
TD |
ASTM D-882 |
64 |
MPa |
||
|
落锤冲击强度 |
|
ASTM D-1709A |
150 |
g |
|
|
1%断裂拉伸模量 |
MD |
ASTM D-882 |
1050 |
MPa |
|
|
TD |
ASTM D-882 |
1100 |
MPa |
||
|
伸长率 |
MD |
ASTM D-882 |
350 |
% |
|
|
TD |
ASTM D-882 |
500 |
% |
||
|
穿刺冲击强度 |
|
ASTM D-1709A |
49 |
J/mm |
|
|
其它性能 |
混浊 |
|
ASTM D-1003 |
70 |
% |
|
分子量分布 |
|
Equate |
宽广 |
|
|