硅灰石以其无毒、无味、无放射性优点,能够取代对人体健康有害的石棉。经过特殊加工工艺后仍能保持其独特的针状结构,使添加了硅灰石针状粉的硅钙板、防火板、纤维水泥板、硫酸钙板等新型环保建筑材料的抗冲击性、抗弯折强度、耐磨强度、防腐蚀、隔热防火性能均大大提高。还可用于白水泥、建筑腻子等方面
ACICULAR POWDER FOR CONSTRUCTION
GRADE :XYNFW-XA |
F-50 F-60 F-65 F-70 |
||||
Chemical Compostion: CaSiO3 |
|||||
CaO |
43-46% |
||||
SiO2 |
48-53% |
||||
Fe2O3 |
≤0.35% |
||||
Al2O3 |
≤0.4% |
||||
MgO |
≤2.0% |
||||
TiO2 |
≤0.02% |
||||
S |
≤0.02% |
||||
P |
≤0.007% |
||||
L.O.I (10500℃) |
≤3.5% |
||||
Sedimentation(ml/30g) |
45-55 |
56-60 |
60-65 |
65-70 |
|
Aspect Ratio(L/D) |
10-15 |
15-18 |
18-20 |
20-25 |
|
Bulk(Tapped) |
0.6-0.7 |
0.4-0.5 |
0.4-0.5 |
0.4-0.5 |
|
Physical Properties: |
|||||
Appearance |
white |
||||
Form |
Acicular |
||||
Mol.wt. |
116 |
||||
Refraction |
1.63 |
||||
PH |
8.9-9.7 |
||||
Hardness (Moths) |
4.5-5.5 |
||||
Expansion Coefficient (mm/mm/'c) |
6.5×10-6
|
||||
Melting Port (0'C) |
1450 |
||||