TPU XL 1092—2原料供应
TPU XL 1092—2
TPU XL 1092—2 颗粒图片
TPU XL 1092—2 原料加工产品展示
TPU XL 1092—2 物性表:
应用领域:
Physical Properties
Metric
English
Comments
Melt Flow
14 g/10 min
@Load 3.80 kg,
Temperature 190 °C
14 g/10 min
@Load 8.38 lb,
Temperature 374 °F
ASTM D1238
52.53 g/10 min
@Load 8.70 kg,
Temperature 190 °C
52.53 g/10 min
@Load 19.2 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties
Metric
English
Comments
Hardness, Shore A
66
66
5 sec. delay; ASTM D2240
Tensile Strength, Ultimate
24.3 MPa
3520 psi
10 in/min; ASTM D412
Elongation at Break
772 %
772 %
10 in/min; ASTM D412
50% Modulus
0.00188 GPa
0.273 ksi
10 in/min; ASTM D412
100% Modulus
0.00245 GPa
0.355 ksi
ISO 37
200% Modulus
0.00315 GPa
0.457 ksi
10 in/min; ASTM D412
300% Modulus
0.00405 GPa
0.587 ksi
10 in/min; ASTM D412
Tear Strength
53.8 kN/m
307 pli
Die 'C' Tear; 20 in/min; ASTM D624
Compression Set
26.9 %
26.9 %
23°C, 22 hrs.; ASTM D395
68 %
@Temperature 70.0 °C
68 %
@Temperature 158 °F
22 hrs; ASTM D395
Tensile Set
12.6 %
12.6 %
23°C, 22 hrs.; at 100% per ASTM D412